A technical analysis of ED copper, VLP copper, and skin-depth physics.
Published: 2026-05-27
1. Physical Principle of the Skin Effect
Under direct current (DC) conditions, current distributes uniformly across the entire cross-section of a copper conductor. However, when alternating current (AC) frequency increases, the constantly changing magnetic field induces eddy currents within the conductor. These eddy currents push the main current toward the outer surface of the conductor.
This phenomenon is known as the skin effect. Its key physical parameter is the skin depth, which defines the thickness of the thin outer layer where current density drops to about 37% of its surface value.
In plain words, the physical law is:
-
The magnitude of skin depth is inversely proportional to the frequency of the AC signal, the conductivity (resistivity) of the material, and the magnetic permeability.
-
In simpler terms: the higher the signal frequency, the smaller the skin depth. This means the effective thickness of copper available for current flow becomes extremely thin.
Variation of Skin Depth with Frequency
As frequency climbs into the gigahertz (GHz) range, the actual thickness of copper that high-frequency signals can utilize shrinks to micrometer or even sub-micrometer levels:
-
At 10 MHz: Skin depth is approximately 20.6 micrometers.
-
At 100 MHz: Skin depth is approximately 6.5 micrometers.
-
At 1 GHz: Skin depth is approximately 2.1 micrometers.
-
At 10 GHz: Skin depth is approximately 0.66 micrometers.
-
At 28 GHz (e.g., 5G or PAM4 signals): Skin depth is only about 0.39 micrometers.
2. Standard Electrolytic Copper (ED Copper)
Manufacturing Process
ED copper foil is manufactured through an electro-deposition process. In a copper sulfate electrolyte bath, copper ions continuously deposit onto a rotating stainless steel cathode drum:
-
Drum Side (Shiny Side): The side pressed against the drum replicates the smooth texture of the drum surface.
-
Matte Side (Bath Side): The side facing the electrolyte, where copper crystals grow naturally outward, forming a rugged, mountainous, and micro-columnar crystal structure.
Surface Micro-topography
Standard ED copper foil exhibits a very pronounced, jagged, tooth-like microscopic profile on its matte side.
-
Surface Roughness (Rz Value): Typically greater than 10 micrometers.
-
Traditional Purpose: In the past, this high roughness was intentional. When laminating the foil with resin in a printed circuit board (PCB), these "copper teeth" would embed deeply into the resin, providing strong mechanical interlocking force to prevent delamination (i.e., high peel strength).
Critical Flaw at High Frequencies
When signal frequency rises (e.g., above 1 GHz), the skin depth becomes much smaller than the surface roughness of the copper foil (10 micrometers). At this point, high-frequency current cannot travel in a straight line; it is forced to follow the steep, jagged "peaks and valleys" of the copper surface.
This significantly lengthens the actual physical path the current must travel. This path elongation and electron scattering caused by surface irregularity leads to severe conductor loss, rapidly attenuating the signal.
3. Very Low Profile Copper Foil (VLP Copper)
Manufacturing Process
VLP copper foil is developed specifically to solve high-frequency losses while maintaining adequate adhesion. It uses special organic grain-refining agents during electrolysis to strictly suppress random crystal growth, or employs post-treatment chemical and mechanical processes to microscopically flatten the surface.
Surface Micro-topography
-
Surface Roughness (Rz Value): Typically controlled between 1.5 and 3.0 micrometers (for advanced HVLP foils, it can be reduced below 1.5 micrometers).
-
Bonding Mechanism: Since there are no large "mechanical teeth," VLP copper foil relies primarily on silane chemical coupling agents and dense micro-nodules to achieve chemical bonding with the resin.
Excellent Performance at High Frequencies
Because the copper surface is significantly "flattened," even at ultra-high frequencies of 10 GHz to 28 GHz (where skin depth is less than 1 micrometer), the current flowing along the surface does not encounter steep obstacles. The current path remains essentially a horizontal straight line, nearly identical to the designed path, thereby minimizing high-frequency conductor loss.
4. Interpretation of Conductor Loss Calculation Models
To evaluate the impact of copper roughness on signals in software simulations (such as PCIe 6.0 or 112G/224G ultra-high-speed channel design), academia and industry have derived correction models. In plain words:
Traditional Hammerstad Roughness Model
This traditional mathematical model assumes that the actual rough loss is equal to the base loss of a perfectly smooth conductor multiplied by an amplification factor determined by the ratio of the root-mean-square roughness to the skin depth.
-
Physical Limitation: This model predicts that loss amplification has an upper limit. When roughness is much larger than skin depth (e.g., ED copper at high frequencies), the loss multiplier tends toward a fixed maximum limit (about 2 times). However, at millimeter-wave or extremely high frequencies, this prediction is often overly optimistic and misses part of the actual loss.
Modern Huray (Snowball) Model
Due to the limitations of the traditional model, modern high-speed digital design prefers the Huray model. Instead of focusing solely on "peak height," this model visualizes the microscopic rough topography of copper foil as a collection of tiny copper spheres stacked on a plane (like snowballs).
-
Physical Logic: It calculates the increase in surface area caused by these micro "snowballs" and combines this with the relationship between skin depth and sphere radius to accumulate the total loss.
-
Analysis Conclusion: ED copper foil is covered with countless large and small "snowballs," causing a drastic expansion of surface area and thus extremely fast high-frequency attenuation. In contrast, VLP copper foil has almost no such large spheres, resulting in minimal surface area increase. This is why VLP ensures perfect signal integrity and reduces signal jitter (Jitter) for high-speed applications.
Summary Comparison Table
-
Surface Roughness:
-
Standard ED Copper: Very High (greater than 10 micrometers)
-
VLP Copper Foil: Extremely Low (1.5 to 3.0 micrometers)
-
-
Bonding Mechanism with Resin:
-
Standard ED Copper: Strong Mechanical Interlocking (Physical Gripping)
-
VLP Copper Foil: Chemical Silane Coupling + Micro Nodules
-
-
Peel Strength (Anti-delamination):
-
Standard ED Copper: Excellent
-
VLP Copper Foil: Moderate to Good
-
-
Performance Under High-Frequency Signals:
-
Standard ED Copper: Exponentially increasing loss beyond 500 MHz
-
VLP Copper Foil: Maintains very low attenuation even at 10 GHz and above
-
-
Core Application Areas:
-
Standard ED Copper: Traditional multilayer PCBs, high-current power boards, DC transmission
-
VLP Copper Foil: 5G/6G RF antennas, high-speed server motherboards, advanced optical transceiver modules
-