What Is Reflow Soldering? Temperature Profiles, Process Steps, and Common Defects
Category: Technical Guides & Design for Manufacturing | Published: 2026-10-30
Reflow soldering is the process that turns a printed circuit board (PCB) and a pile of surface-mount components into a working assembly. A sticky solder paste—a mix of tiny metal particles and flux—is printed onto the board, components are placed on top, and the whole board travels through a reflow oven. Inside the oven, a carefully controlled temperature profile melts the alloy so that it wets the pads and component leads, then cools and solidifies into a permanent joint.
For anyone sourcing or specifying a PCB assembly service, understanding this process matters. The quality of every joint depends less on the oven itself than on the temperature curve it follows.
How Reflow Soldering Fits Into SMT Assembly
Reflow is one stage in a wider surface-mount technology (SMT) line. Before a board reaches the oven, solder paste stencil printing deposits a precise amount of paste onto every pad, and a pick-and-place machine sets each component in position. Too much or too little paste at this stage cannot be corrected later, which is why many lines add a solder paste inspection (SPI) system immediately after printing.
Once placement is complete, the board enters the reflow oven. The oven does not simply “get hot.” It moves the board through a sequence of temperature zones so that flux can activate, solvents can evaporate, and the alloy can melt and cool in a controlled way. After reflow, defects are checked by AOI inspection, and in the case of hidden joints such as ball grid arrays (BGAs), by X-ray inspection.
The Four Stages of a Reflow Profile
A reflow profile is the temperature history measured at the solder joint, not the temperature shown on the oven panel. Engineers record it with a thermal profiler, following IPC-7530 thermal profiling guidance.
1. Preheat (Ramp)
The board warms at a controlled rate, typically 1–3°C per second, up to about 150°C. This removes ambient moisture and prepares the assembly for the soak stage without shocking components or the board.
2. Soak (Equilibrium)
In the 150–200°C range, the board is held for roughly 60–120 seconds. Soak evens out temperature across large and small components, activates the flux, and allows volatiles to escape before the alloy melts. Uneven soaking is a common cause of defects such as tombstoning.
3. Reflow (Peak)
Temperature rises past the liquidus. For the common lead-free alloy SAC305, the liquidus is 217°C, and the recommended peak sits between 235°C and 245°C. The time above liquidus (TAL) should be about 45–90 seconds. These values come from the paste manufacturer’s datasheet as well as IPC recommendations, and they leave only a narrow process window of roughly 35°C.
4. Cooling
The board cools at 2–4°C per second. Controlled cooling produces a fine, strong grain structure in the joint. Cooling too slowly encourages large grains and brittle joints; cooling too quickly can cause component stress.
Lead-Free vs. Tin-Lead Profiles
Not every line uses SAC305. Legacy or specialist products may still use a tin-lead alloy such as Sn63/Pb37, whose liquidus is 183°C and whose typical peak range is 205–220°C.
|
Parameter |
SAC305 (Lead-Free) |
Sn63/Pb37 (Tin-Lead) |
|---|---|---|
|
Liquidus |
217°C |
183°C |
|
Peak temperature |
235–245°C |
205–220°C |
|
Time above liquidus |
45–90 s |
45–75 s |
|
Ramp rate |
1–3°C/s |
1–3°C/s |
|
Cooling rate |
2–4°C/s |
2–4°C/s |
Mixed assemblies require extra care because the two alloys melt at different temperatures. Nitrogen reflow, which reduces oxidation and improves wetting, is often used for fine-pitch and BGA packages, though it adds cost and does not replace correct profile settings.
Process Steps in Detail
- Solder paste printing – A stainless-steel stencil deposits paste through laser-cut apertures. Aperture size, stencil thickness, and print pressure decide paste volume.
- SPI and component placement – Paste volume is verified, then components are placed by a high-speed pick-and-place machine.
- Reflow heating – The board passes through preheat, soak, reflow, and cooling zones inside the oven.
- Inspection – AOI catches visible defects, while X-ray inspection finds voids and head-in-pillow defects under BGAs.
Common Reflow Defects and Causes
|
Defect |
Root Cause |
Profile or Process Fix |
|---|---|---|
|
Tombstoning |
Uneven pad heating or paste volume |
Extend soak; balance pad sizes |
|
Bridging |
Excess paste, fine-pitch pads |
Reduce aperture; optimise peak |
|
Solder balls |
Fast ramp or damp paste |
Slow preheat; check storage |
|
Cold joint |
Peak too low or TAL too short |
Raise peak 3–5°C; extend TAL |
|
Voids (BGA) |
Trapped flux gas |
Extend soak; use low-void paste |
|
Head-in-pillow |
BGA warpage during reflow |
Review profile; check package |
A profile must be validated for every new board design because copper area, board thickness, and component mix all change how a board absorbs heat.
Moisture Sensitivity and Storage
Components such as BGAs and moisture-sensitive devices (MSLs) absorb ambient moisture. If a moist component enters the oven, rapid heating can cause internal steam pressure, leading to package cracking known as the “popcorn effect.” Follow J-STD-020 for floor life and J-STD-033 for baking and dry-pack handling.
Conclusion
Reflow soldering looks simple—heat the board until the solder melts—but consistent results depend on a validated temperature profile, correct paste volume, and proper storage of moisture-sensitive parts. Whether you are reviewing SAC305 lead-free solder paste for a new design or specifying an SMT pick-and-place machine for higher volume, the profile is where good joints are won or lost.
Frequently Asked Questions
What temperature is used for reflow soldering?
For lead-free SAC305, the peak is 235–245°C with a liquidus of 217°C. Tin-lead Sn63/Pb37 peaks at 205–220°C with a liquidus of 183°C.
What is time above liquidus (TAL)?
TAL is the number of seconds that the joint temperature stays above the alloy’s liquidus. For SAC305, 45–90 seconds is typical.
What causes tombstoning during reflow?
Tombstoning usually comes from uneven heating between the two pads of a small component, often made worse by unequal pad size or paste volume.
How is a reflow profile measured?
A thermal profiler attaches thermocouples to key joints on the board and records temperature throughout the oven run, following IPC-7530 thermal profiling guidance.